Table 3 The energy degrading foils characteristics for Aluminum, Molybdenum and Havar

From: Efficiency of 124I radioisotope production from natural and enriched tellurium dioxide using 124Te(p,xn)124I reaction

Property

Aluminum

Molybdenum

Havar

Thermal conductivity (W m−1 K−1)

167

138

13

Melting point (°C)

582

2620

1480

Density (g cm−3)

2.7

10.2

8.3